Phosphate High Alumina Mortar
AL2O3 Min70%
Refractoriness Min1790C
Sticking time 1-3min
Grain size,+0.5mm Max2
-0.074 Min50
Bonding MOR,MPa 110C*24h Min1.96
1400C*3h Min5.9
Application For laying property-modified high alumina brick
|
|
|
|
| |
|
|
|