Model Number |
WNM |
WNM-1 WNM-2 WNM-3
AL2O3,% Min80 Min75 Min70
SiO2,% Max15 Max20 Max25
BD,g/cm3 Min2.9 Min2.8 Min2.7
CCS,MPa Min100 Min85 Min70
CMOR,MPa Min15.2 Min13.6 Min11
Abrasion loss Max5.8cm3 Max8.3cm3 Max9.6cm3
Refractories temp Min1790C Min1790C Min1790C
RUL 0.20MPa Min1550C Min1530C Min1500C
TC,W/m.K Max1.49 Max1.49 Max1.49
TSR Min20 Min20 Min20
Max service temp Min1650C Min1600C Min1500C
Application Cooling zone and burning zone of cement rotary kiln and AL-making rotary kiln.
|